Hello,
I'm at the stage now where I am rubbing back all of the tatty bit's on the underside of my Cossie before paint.
On the spare wheel bowl (under car) after I rubbed it back, it has slight pitting on the metal.
Am I right in thinking - Acid etch then High Build primer over the pitted areas then rub back?
It's just, I was told from the paint supllier to put body colour onto acid ecth after around 4-6 hours whilst it was still tacky and before it cures?
I'm at the stage now where I am rubbing back all of the tatty bit's on the underside of my Cossie before paint.
On the spare wheel bowl (under car) after I rubbed it back, it has slight pitting on the metal.
Am I right in thinking - Acid etch then High Build primer over the pitted areas then rub back?
It's just, I was told from the paint supllier to put body colour onto acid ecth after around 4-6 hours whilst it was still tacky and before it cures?
if i were u i would remove all the rust
then apply 2 coats of epoxy primer seam seal all seams then smoth stone chip then paint
dont know what your suplier is on about lol etch is ment to be a mist coat to seal moisture then apply 2k primer over it
then apply 2 coats of epoxy primer seam seal all seams then smoth stone chip then paint
dont know what your suplier is on about lol etch is ment to be a mist coat to seal moisture then apply 2k primer over it
Last edited by xr3iturbo; Aug 10, 2010 at 07:34 PM.