View Single Post
Old Oct 15, 2013 | 09:00 PM
  #2  
PAUL V's Avatar
PAUL V
Too many posts.. I need a life!!
20 Year Member
Liked
 
Joined: May 2004
Posts: 788
Likes: 4
From: shropshire
Default

Tried is and could not get constant results, You really need to devote a lot of time to building a proper rigg and not just a plastic bucket that you get sold.

You need a to keep the solution "clean" and at the right temp the same with the voltage / amps.

Not saying it can not be done but i found it cheaper easier to sub it out like chroming.

Have a look on this forum
http://forum.caswellplating.com/
Reply