Originally Posted by
whizzisat114
i was gonna say mix it 2-1 to make it a little less viscous then mix the last coat 1-1
and put a slightly dryer coat on to lay the mettalic down a little more even.
i would help you if you'd of used a tintable primer
massive thanks to you for that on using a tintable primmer i will ask about that next time ive been spraying for 18 years and havent come across this problem...
ive done 2-1 mix aswell and that still took 6 coats im going to give it another go monday before i say fook it and give up..
i will use an undercoat (blue) and then see what happends from there...