It's a shame as the paint looks really well done, but I was going to say as soon as I saw the side molding smoothing thats going to crack/fall out. An area that big/deep needs a plate welding in and skimming rather than filled with fibreglass/filler. It doesn't even look like they took it down to bare metal which you should with large areas like that, especially on doors which will be slammed shut.