Originally Posted by BigErn
Im intrigued by this dry flatting hi build primer with 240 and 320. We always wet flat with 400 and 800, be it for solid colour or basecoat. Clearcoat is wet flatted and nibbed with 1500 then go over it again with 2000 before polishing.