Originally Posted by tabetha
Is actually lead, called lead loading way better than filler as does not shrink or react with anything.
It cools so quick when it hits cold metal(body) it does not run, then is filed to shape, VERY VERY expensive way to do it.
tabetha
u have to cover ther area with tin before you add the lead. this process is called tinning. lead filling is a dying trade thou. its not very safe and its not really used within the body repair trade anymore